TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 3 PHR Varox DBPH-50

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 3 PHR Varox DBPH-50.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is carried out by the use of various peroxides including dicumyl peroxide (DCP) or 2,5-dimethyl-2,5-bis (t-butylperoxy) hexane (DBPH).FormulationMillathane 5004100Stearic Acid0.25Hi-Sil 23320Varox DBPH-503All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
Tensile Strength, Yield 28.8 MPa
4170 psi
Elongation at Yield 570 %
570 %
300% Modulus 0.00800 GPa
1.16 ksi
Tear Strength 68.3 kN/m
390 pli
ASTM Die C
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 152 °C
1.00 hour

@Temperature 305 °F