Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 0.0 PHR MBT

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer TSE Industries, Inc
Trade Name Millathane®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 0.0 PHR MBT.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and many other high performance polyurethane applications. Millathane 76 can be vulcanized by sulfur or peroxide cured systems.The combination of thiazole accelerators, MBTS and MBT, enable the best possible cure for Millathane® 76. An increase in MBTS results in a higher state of cure and increased processing safety.An increase in MBT decreases scorch time and increases the state of cure.All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 63
63
Tensile Strength, Yield 30.1 MPa
4370 psi
Elongation at Yield 615 %
615 %
100% Modulus 0.00290 GPa
0.420 ksi
200% Modulus 0.00641 GPa
0.930 ksi
300% Modulus 0.01134 GPa
1.645 ksi
Tear Strength 60.4 kN/m
345 pli
Die C
Compression Set 36 %

@Temperature 70.0 °C,
Time 79200 sec
36 %

@Temperature 158 °F,
Time 22.0 hour
Processing Properties Metric English Comments
Cure Time 6.40 min

@Temperature 155 °C
0.107 hour

@Temperature 311 °F
ts2
12.0 min

@Temperature 155 °C
0.200 hour

@Temperature 311 °F
TC90