Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Non-Black, Aerosil 200

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Non-Black, Aerosil 200.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and many other high performance polyurethane applications. Millathane 76 can be vulcanized by sulfur or peroxide cured systems.FormulationMillathane 76 100.0Zinc Stearate0.5Poly AC 617A1.0MBTS4.0MBT2.0Thanecure® ZM1.0TP-9510.0Sulfur2.0Aerosil 20020All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 57
57
Tensile Strength, Yield 32.53 MPa
4718 psi
Elongation at Yield 699 %
699 %
100% Modulus 0.00135 GPa
0.196 ksi
200% Modulus 0.00230 GPa
0.333 ksi
300% Modulus 0.00379 GPa
0.549 ksi
Tear Strength 44.7 kN/m
255 pli
Taber Abrasion, mg/1000 Cycles 5.0

@Load 1.00 kg
5.0

@Load 2.20 lb
H-18 wheel
Compression Set 50.8 %

@Temperature 70.0 °C,
Time 79200 sec
50.8 %

@Temperature 158 °F,
Time 22.0 hour
Processing Properties Metric English Comments
Cure Time 10.0 min

@Temperature 155 °C
0.167 hour

@Temperature 311 °F