TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.5 PHR Varox DBPH-50 Peroxide

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer TSE Industries, Inc
Trade Name Millathane®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.5 PHR Varox DBPH-50 Peroxide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and many other high performance polyurethane applications. Millathane 76 can be vulcanized by sulfur or peroxide cured systems.Curing of Millathane®76 can easily be done with many types of peroxides. Millathane76 peroxide vulcanizates have superior compression set, greater heat stability, and are more resistant to reversion than sulfur cures.FormulationVarox DBPH-502.5Millathane 76100.0Stearic Acid0.25Poly AC 617A0.5N-55035.0TP-953.0All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 66
66
70
70
heat aged 70 hours @ 100ºC
Tensile Strength, Yield 24.14 MPa
3501 psi
27.11 MPa
3932 psi
heat aged 70 hours @ 100ºC
Elongation at Yield 269 %
269 %
heat aged 70 hours @ 100ºC
289 %
289 %
100% Modulus 0.00472 GPa
0.684 ksi
200% Modulus 0.0155 GPa
2.25 ksi
Tear Strength 51.0 kN/m
291 pli
Die C
Compression Set 28.2 %

@Temperature 100 °C,
Time 79200 sec
28.2 %

@Temperature 212 °F,
Time 22.0 hour
Processing Properties Metric English Comments
Cure Time 7.00 min

@Temperature 83.3 °C
0.117 hour

@Temperature 182 °F