Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 40 PHR Carbon Black, N-550 (FEF)

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer TSE Industries, Inc
Trade Name Millathane®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 40 PHR Carbon Black, N-550 (FEF).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and many other high performance polyurethane applications. Millathane 76 can be vulcanized by sulfur or peroxide cured systems.FormulationMillathane 76 100.0Zinc Stearate0.5Poly AC 617A1.0TP-9510.0Thanecure® ZM1.0MBTS4.0MBT2.0Sulfur1.5N-55040All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
Tensile Strength, Yield 23.67 MPa
3433 psi
Elongation at Yield 490 %
490 %
100% Modulus 0.00459 GPa
0.666 ksi
200% Modulus 0.009915 GPa
1.438 ksi
300% Modulus 0.01623 GPa
2.354 ksi
Tear Strength 60.6 kN/m
346 pli
Taber Abrasion, mg/1000 Cycles 4.0

@Load 1.00 kg
4.0

@Load 2.20 lb
H-18 wheel
Compression Set 43.3 %

@Temperature 70.0 °C,
Time 79200 sec
43.3 %

@Temperature 158 °F,
Time 22.0 hour
Processing Properties Metric English Comments
Cure Time 10.0 min

@Temperature 154 °C
0.167 hour

@Temperature 309 °F
Users viewing this material also viewed the following: