Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 70A, Non-Black Peroxide Cure.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and many other high performance polyurethane applications. Millathane 76 can be vulcanized by sulfur or peroxide cured systems.FormulationMillathane 76 100.0Stearic Acid0.5Hi-Sil 23330.0Sartomer SR-2973.0Di-Cup 40C2.0All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
Tensile Strength, Yield 24.5 MPa
3560 psi
Elongation at Yield 386 %
386 %
100% Modulus 0.00331 GPa
0.480 ksi
200% Modulus 0.00678 GPa
0.984 ksi
300% Modulus 0.01420 GPa
2.059 ksi
Tear Strength 44.8 kN/m
256 pli
Die C
Processing Properties Metric English Comments
Cure Time 15.0 min

@Temperature 160 °C
0.250 hour

@Temperature 320 °F