TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 90A, Non-Black Peroxide Cure

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer TSE Industries, Inc
Trade Name Millathane®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 90A, Non-Black Peroxide Cure.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and many other high performance polyurethane applications. Millathane 76 can be vulcanized by sulfur or peroxide cured systems.FormulationMillathane 76 100.0Stearic Acid0.5Poly-AC 617A2.0Hi-Sil 23360.0SR-2977.5Di-Cup 40C3.0Diethyleneglycol1.0All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
Tensile Strength, Yield 17.71 MPa
2568 psi
Elongation at Yield 300 %
300 %
100% Modulus 0.007846 GPa
1.138 ksi
200% Modulus 0.01196 GPa
1.735 ksi
300% Modulus 0.01771 GPa
2.568 ksi
Tear Strength 58.07 kN/m
331.3 pli
Die C
Processing Properties Metric English Comments
Cure Time 7.00 min

@Temperature 155 °C
0.117 hour

@Temperature 311 °F