Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 90A, Non-Black Sulfur Cure

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 90A, Non-Black Sulfur Cure.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and many other high performance polyurethane applications. Millathane 76 can be vulcanized by sulfur or peroxide cured systems.FormulationMillathane 76 100.0Zinc Stearate0.5Mistron Vapor60.0Cumar P105.0Hi-Sil 23330.0Pliolite S6B10.0MBTS4.0MBT2.0Thanecure® ZM1.0Sulfur2.0All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
Tensile Strength, Yield 12.5 MPa
1810 psi
Elongation at Yield 510 %
510 %
100% Modulus 0.00501 GPa
0.726 ksi
200% Modulus 0.00671 GPa
0.973 ksi
300% Modulus 0.00786 GPa
1.14 ksi
Tear Strength 56.4 kN/m
322 pli
Die C
Processing Properties Metric English Comments
Cure Time 15.0 min

@Temperature 155 °C
0.250 hour

@Temperature 311 °F
Users viewing this material also viewed the following: