TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, Hardness 62A

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, Hardness 62A.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed for applications in shoe soling, roll coverings and all other applications where transparent, brightly colored or decorative products are desired.FormulationMillathane 97 100Stearic Acid0.25Wacker HDK-N2020Irganox 10100.25SR-231 (DEGDMA)3Luperox 2310.4All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 62
62
Tensile Strength, Yield 22.59 MPa
3277 psi
Elongation at Yield 555 %
555 %
100% Modulus 0.00160 GPa
0.232 ksi
200% Modulus 0.00220 GPa
0.319 ksi
300% Modulus 0.00340 GPa
0.493 ksi
Tear Strength 30.5 kN/m
174 pli
Die C
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Processing Properties Metric English Comments
Cure Time 8.00 min

@Temperature 149 °C
0.133 hour

@Temperature 300 °F