TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, Hardness 70A

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer TSE Industries, Inc
Trade Name Millathane®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, Hardness 70A.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed for applications in shoe soling, roll coverings and all other applications where transparent, brightly colored or decorative products are desired.FormulationMillathane 97 100Stearic Acid0.5Wacker HDK-N2030Silquest A-1720.3Irganox 10100.25SR-231 (DEGDMA)3Luperox 2310.5All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
Tensile Strength, Yield 26.55 MPa
3851 psi
Elongation at Yield 462 %
462 %
100% Modulus 0.00234 GPa
0.339 ksi
200% Modulus 0.00506 GPa
0.734 ksi
300% Modulus 0.009839 GPa
1.427 ksi
Tear Strength 34.5 kN/m
197 pli
Die C
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Processing Properties Metric English Comments
Cure Time 6.00 min

@Temperature 149 °C
0.100 hour

@Temperature 300 °F