TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 1.0 PHR Sulfur

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer TSE Industries, Inc
Trade Name Millathane®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 1.0 PHR Sulfur.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outstanding hydrolytic stability and improved processing. MILLATHANE E34 can be compounded and processed by the use of conventional rubber manufacturing equipment — mixed on two roll mills or an internal mixer. Compounds can be — calendered; extruded; injection, transfer, or compression molded — to produce finished polyurethane parts. It can be vulcanized by organic peroxides or sulfur with thiazole accelerators.FormulationMillathane E34100Zinc Stearate0.5N330 Black30.0Cumar P1010.0MBTS4.0MBT2.0Thanecure® ZM1.0Sulfur1.0All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A >= 64
>= 64
Tensile Strength, Yield 29.19 MPa
4234 psi
Elongation at Yield 562 %
562 %
100% Modulus 0.00260 GPa
0.377 ksi
200% Modulus 0.00560 GPa
0.812 ksi
300% Modulus 0.009797 GPa
1.421 ksi
Tear Strength 35.2 kN/m
201 pli
Die C
Compression Set 32 %

@Temperature 70.0 °C,
Time 79200 sec
32 %

@Temperature 158 °F,
Time 22.0 hour
Processing Properties Metric English Comments
Cure Time 12.5 min

@Temperature 155 °C
0.208 hour

@Temperature 311 °F