Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 60 PHR N220 (ISAF) Filler

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer TSE Industries, Inc
Trade Name Millathane®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 60 PHR N220 (ISAF) Filler.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outstanding hydrolytic stability and improved processing. MILLATHANE E34 can be compounded and processed by the use of conventional rubber manufacturing equipment — mixed on two roll mills or an internal mixer. Compounds can be — calendered; extruded; injection, transfer, or compression molded — to produce finished polyurethane parts. It can be vulcanized by organic peroxides or sulfur with thiazole accelerators.FormulationMillathane E34100.0Zinc Stearate0.5Struktol WB 2220.5Poly AC 617A0.5Cumar P1010.0MBTS4.0MBT2.0Thanecure® ZM1.0Sulfur1.5Carbon Black N-220 (ISAF)60All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A >= 80
>= 80
Tensile Strength, Yield 24.90 MPa
3611 psi
Elongation at Yield 442 %
442 %
100% Modulus 0.007598 GPa
1.102 ksi
200% Modulus 0.01530 GPa
2.219 ksi
300% Modulus 0.02050 GPa
2.973 ksi
Tear Strength 36.0 kN/m
205 pli
Die C
Processing Properties Metric English Comments
Cure Time 10.0 min

@Temperature 68.3 °C
0.167 hour

@Temperature 155 °F
Press cured
Descriptive Properties Value Comments
DIN Abrasion (mm³) 43.2