Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 20 PHR Dixie Clay Filler

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer TSE Industries, Inc
Trade Name Millathane®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 20 PHR Dixie Clay Filler.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear strength, oil and fuel resistance, and ozone resistance. The life expectancy of urethane is often 5 times longer than other elastomers, thus saving material costs and downtime expense. One shortcoming of polyurethanes is loss of physical properties at temperatures over 180°F (82°C). MILLATHANE HT has overcome this weakness.FormulationMillathane HT100.0Zinc Stearate0.5MBTS4.0MBT2.0THANECURE® ZM1.0Sulfur1.5Dixie Clay20All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 54
54
Tensile Strength, Yield 19.71 MPa
2858 psi
Elongation at Yield 456 %
456 %
100% Modulus 0.00252 GPa
0.365 ksi
200% Modulus 0.00584 GPa
0.847 ksi
300% Modulus 0.009253 GPa
1.342 ksi
Tear Strength 35.4 kN/m
202 pli
Die C
Compression Set 58 %

@Temperature 70.0 °C,
Time 79200 sec
58 %

@Temperature 158 °F,
Time 22.0 hour
Processing Properties Metric English Comments
Cure Time 19.0 min

@Temperature 154 °C
0.317 hour

@Temperature 310 °F
Press cured