Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 2.0 PHR MBTS

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 2.0 PHR MBTS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear strength, oil and fuel resistance, and ozone resistance. The life expectancy of urethane is often 5 times longer than other elastomers, thus saving material costs and downtime expense. One shortcoming of polyurethanes is loss of physical properties at temperatures over 180°F (82°C). MILLATHANE HT has overcome this weakness.An increase in the level of MBTS results in more processing safety, plus it gives a higher state of cure. On the other hand, MBT acts as an accelerator which, when increased, will cause a decrease in processing safety and a higher state of cure.All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 81
81
Tensile Strength, Yield 18.75 MPa
2719 psi
Elongation at Yield 517 %
517 %
100% Modulus 0.00418 GPa
0.606 ksi
200% Modulus 0.008991 GPa
1.304 ksi
300% Modulus 0.0137 GPa
1.99 ksi
Tear Strength 48.0 kN/m
274 pli
Die C
Compression Set 63 %

@Temperature 70.0 °C,
Time 79200 sec
63 %

@Temperature 158 °F,
Time 22.0 hour
Processing Properties Metric English Comments
Cure Time 7.00 min

@Temperature 160 °C
0.117 hour

@Temperature 320 °F
Press cured
Descriptive Properties Value Comments
DIN Abrasion (mm³) 124
Copyright © lookpolymers.com All Rights Reserved