Taiwan PU Corporation TPUI-T95 Transparent Grade, Injection Molding Polyester Base TPU

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Taiwan PU Corporation
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Taiwan PU Corporation TPUI-T95 Transparent Grade, Injection Molding Polyester Base TPU.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Thermoplastic Polyurethane (TPU), Transparent Grade, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation.
Mechanical Properties Metric English Comments
Hardness, Shore A 95
95
Tensile Strength at Break 38.25 MPa
5548 psi
Elongation at Break 550 %
550 %
100% Modulus 0.0118 GPa
1.71 ksi
300% Modulus 0.0186 GPa
2.70 ksi
Resilience 30
30
%, Impact Resilience
Taber Abrasion, mg/1000 Cycles 15
15
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Processing Properties Metric English Comments
Feed Temperature 190 °C
374 °F
Middle Barrel Temperature 195 °C
383 °F
Compress zone
Front Barrel Temperature 200 °C
392 °F
Metering zone
Adapter Temperature 205 °C
401 °F
Die Temperature 205 °C
401 °F