Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Taiwan Sheen Soon Sheenthane® A9312R Thermoplastic Polyurethane Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane TPE , Polyurethane, TP
Manufacturer Taiwan Sheen Soon Co. Ltd.
Trade Name Sheenthane®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Taiwan Sheen Soon Sheenthane® A9312R Thermoplastic Polyurethane Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
Mechanical Properties Metric English Comments
Hardness, Shore A 91 - 95
91 - 95
Tensile Strength 34.3 MPa
4980 psi
Elongation at Break 500 %
500 %
100% Modulus 0.007343 GPa
1.065 ksi
300% Modulus 0.0137 GPa
1.99 ksi
Processing Properties Metric English Comments
Processing Temperature 175 - 195 °C
347 - 383 °F