Taiwan Sheen Soon Sheenthane® D6010E Thermoplastic Polyurethane Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane TPE , Polyurethane, TP
Manufacturer Taiwan Sheen Soon Co. Ltd.
Trade Name Sheenthane®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Taiwan Sheen Soon Sheenthane® D6010E Thermoplastic Polyurethane Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD.
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
Mechanical Properties Metric English Comments
Hardness, Shore D 60 - 64
60 - 64
Tensile Strength 53.9 MPa
7820 psi
Elongation at Break 350 %
350 %
100% Modulus 0.0245 GPa
3.55 ksi
300% Modulus 0.0441 GPa
6.40 ksi
Processing Properties Metric English Comments
Processing Temperature 190 - 210 °C
374 - 410 °F