Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.45 g/cc
1.45 g/cc
ASTM D792
Water Absorption 0.25 %
0.25 %
24 Hrs; ASTM D570
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 110 MPa
16000 psi
ASTM D638
Tensile Modulus 11.4 GPa
1650 ksi
ASTM D638
Flexural Strength 152 MPa
22000 psi
ASTM D790
Flexural Modulus 11.0 GPa
1600 ksi
ASTM D790
Izod Impact, Notched 0.374 J/cm
0.700 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 166 °C
330 °F
ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1.0 - 10 ohm-cm
1.0 - 10 ohm-cm
ASTM D648
Surface Resistivity per Square 1.0 - 10 ohm
1.0 - 10 ohm
ASTM D648
Users viewing this material also viewed the following: