Techmer ES HiFill® ABS 0350

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded
Manufacturer Techmer ES
Trade Name HiFill®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill® ABS 0350.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaFeatures: High DensityForms: PelletsProcessing Method: Extrusion MoldingInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 3.50 g/cc
0.126 lb/in³
ASTM D792
Water Absorption 0.025 %

@Time 86400 sec
0.025 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 cm/cm
0.0050 in/in
ASTM D955
Melt Flow 0.80 g/10 min

@Load 3.80 kg,
Temperature 230 °C
0.80 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 95
95
ASTM D785
Tensile Strength 24.1 MPa
3500 psi
ASTM D638
Elongation at Break 40 %
40 %
ASTM D638
Flexural Strength 26.9 MPa
3900 psi
ASTM D790
Flexural Modulus 0.0241 GPa
3.50 ksi
ASTM D790
Izod Impact, Notched 1.60 J/cm

@Thickness 3.17 mm
3.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 79.4 °C
175 °F
Unannealed; ASTM D648