Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Mica Filler, 40% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.29 g/cc
0.0466 lb/in³
ASTM D792
Water Absorption 0.050 %

@Time 86400 sec
0.050 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0040 cm/cm

@Thickness 3.17 mm
0.0040 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 112
112
ASTM D785
Tensile Strength, Yield 33.1 MPa
4800 psi
ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Flexural Strength 42.7 MPa
6200 psi
ASTM D790
Flexural Modulus 5.17 GPa
750 ksi
ASTM D790
Izod Impact, Notched 0.854 J/cm

@Thickness 3.17 mm
1.60 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 34.2 µm/m-°C
19.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 143 °C
290 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 116 °C
240 °F
Unannealed; ASTM D648