Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES HiFill® PP CO GF43 CC 43% Glass Filled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer , Polypropylene with 40% Glass Fiber Filler
Manufacturer Techmer ES
Trade Name HiFill®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill® PP CO GF43 CC 43% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 43% Filler by WeightFeatures: Copolymer and Chemically CoupledInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ASTM D792
Water Absorption 0.050 %

@Time 86400 sec
0.050 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.035 cm/cm

@Thickness 3.17 mm
0.035 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ASTM D785
Tensile Strength, Yield 75.8 MPa
11000 psi
ASTM D638
Elongation at Break 5.5 %
5.5 %
ASTM D638
Flexural Strength 128 MPa
18500 psi
ASTM D790
Flexural Modulus 7.24 GPa
1050 ksi
ASTM D790
Izod Impact, Notched 2.08 J/cm

@Thickness 3.17 mm
3.90 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 37.8 µm/m-°C
21.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 157 °C
315 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 132 °C
270 °F
Unannealed; ASTM D648
Flammability, UL94 HB
HB