Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ASTM D792
Water Absorption 0.050 %

@Time 86400 sec
0.050 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0030 cm/cm

@Thickness 3.17 mm
0.0030 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 112
112
ASTM D785
Tensile Strength, Yield 86.2 MPa
12500 psi
ASTM D638
Elongation at Yield 3.0 %
3.0 %
ASTM D638
Flexural Yield Strength 141 MPa
20500 psi
ASTM D790
Flexural Modulus 7.58 GPa
1100 ksi
ASTM D790
Izod Impact, Notched 1.17 J/cm

@Thickness 3.17 mm
2.20 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 6.94 J/cm

@Thickness 3.17 mm
13.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 27.0 µm/m-°C
15.0 µin/in-°F
ASTM D696
Melting Point 163 °C
325 °F
Deflection Temperature at 0.46 MPa (66 psi) 163 °C
325 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 154 °C
310 °F
Unannealed; ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 3.00e+16 ohm-cm
3.00e+16 ohm-cm
ASTM D257
Dielectric Strength 20.5 kV/mm
520 kV/in
Method A (Short-Time); ASTM D149