Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES HiFill® TPX-PVDF-03009 C

Category Polymer , Thermoplastic , Fluoropolymer , PVDF
Manufacturer Techmer ES
Trade Name HiFill®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill® TPX-PVDF-03009 C.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral FillerFeatures: Low Shrinkage and Low Smoke EmissionInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.79 g/cc
0.0647 lb/in³
ASTM D792
Water Absorption 0.020 %

@Time 86400 sec
0.020 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.021 cm/cm

@Thickness 3.17 mm
0.021 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 104
104
ASTM D785
Tensile Strength, Yield 37.2 MPa
5400 psi
ASTM D638
Elongation at Break 40 %
40 %
ASTM D638
Flexural Yield Strength 60.7 MPa
8800 psi
ASTM D790
Flexural Modulus 2.83 GPa
410 ksi
ASTM D790
Izod Impact, Notched 1.12 J/cm

@Thickness 3.17 mm
2.10 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 72.0 µm/m-°C
40.0 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 157 °C
315 °F
Unannealed; ASTM D648
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
ASTM D257