Techmer ES Luriblend® PA4/6 HS TL15

Category Polymer , Thermoplastic , Nylon , Nylon 46
Manufacturer Techmer ES
Trade Name Luriblend®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Luriblend® PA4/6 HS TL15.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and PTFE Lubricant (15%)Features: Heat Stabilized and LubricatedUL File Number: E157318Information provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.27 g/cc
0.0459 lb/in³
ASTM D792
Water Absorption 1.2 %

@Time 86400 sec
1.2 %

@Time 24.0 hour
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ASTM D785
Tensile Strength, Yield 58.6 MPa
8500 psi
ASTM D638
Elongation at Yield 300 %
300 %
ASTM D638
Flexural Yield Strength 62.1 MPa
9000 psi
ASTM D790
Flexural Modulus 1.21 GPa
175 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm

@Thickness 3.17 mm,
Temperature -40.0 °C
1.00 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
2.94 J/cm

@Thickness 3.17 mm,
Temperature 72.8 °C
5.50 ft-lb/in

@Thickness 0.125 in,
Temperature 163 °F
ASTM D256
Izod Impact, Unnotched NB

@Thickness 3.17 mm
NB

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 79.2 µm/m-°C
44.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 221 °C
430 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
ASTM D257
Dielectric Strength 21.7 kV/mm
550 kV/in
Method A (Short-Time); ASTM D149