Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES Luriblend® PA6/10 GF30 TS15 30% Glass Filled

Category Polymer , Thermoplastic , Nylon , Nylon 610 , Nylon 610, Glass Reinforced
Manufacturer Techmer ES
Trade Name Luriblend®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Luriblend® PA6/10 GF30 TS15 30% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer and PTFE+ Silicone LubricantFeatures: Lubricated, Heat Stabilizer and Good Wear ResistanceInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.43 g/cc
0.0517 lb/in³
ASTM D792
Water Absorption 0.16 %

@Time 86400 sec
0.16 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 cm/cm

@Thickness 3.17 mm
0.0050 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 117 MPa
17000 psi
ASTM D638
Elongation at Yield 4.0 %
4.0 %
ASTM D638
Flexural Yield Strength 195 MPa
28300 psi
ASTM D790
Flexural Modulus 7.58 GPa
1100 ksi
ASTM D790
Izod Impact, Notched 1.12 J/cm

@Thickness 3.17 mm
2.10 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 8.54 J/cm

@Thickness 3.17 mm
16.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 27.0 µm/m-°C
15.0 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 207 °C
405 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
ASTM D257