Techmer ES Luriblend® PC GF30 TS15 BK 30% Glass Filled

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, 30% Glass Filled , Polycarbonate, PTFE Filled
Manufacturer Techmer ES
Trade Name Luriblend®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Luriblend® PC GF30 TS15 BK 30% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: PTFE + Silicone LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ASTM D792
Water Absorption 0.060 %

@Time 86400 sec
0.060 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0030 cm/cm

@Thickness 3.17 mm
0.0030 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 116
116
ASTM D785
Tensile Strength, Yield 75.8 MPa
11000 psi
ASTM D638
Elongation at Break 3.5 %
3.5 %
ASTM D638
Flexural Yield Strength 96.5 MPa
14000 psi
ASTM D790
Flexural Modulus 4.55 GPa
660 ksi
ASTM D790
Izod Impact, Notched 0.427 J/cm

@Thickness 3.17 mm
0.800 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 28.8 µm/m-°C
16.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 182 °C
360 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 132 °C
270 °F
Unannealed; ASTM D648
Users viewing this material also viewed the following: