Techmer ES Luriblend® TPU 40D GL10

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer Techmer ES
Trade Name Luriblend®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Luriblend® TPU 40D GL10.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsAdditive: Graphite Powder Lubricant(10%)Features: LubricatedInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.18 g/cc
0.0426 lb/in³
ASTM D792
Water Absorption 0.20 %

@Time 86400 sec
0.20 %

@Time 24.0 hour
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Shore D 40
40
ASTM D2240
Tensile Strength at Break 40.0 MPa
5800 psi
ASTM D638
Elongation at Break 580 %
580 %
ASTM D638
100% Modulus 0.00552 GPa
0.800 ksi
ASTM D412
Tear Strength 105 kN/m
600 pli
ASTM D624
Thermal Properties Metric English Comments
Vicat Softening Point 85.0 °C
185 °F
ASTM D1525