Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES Plaslube® AC-80/TF/15 Acetal (Copolymer), 15% PTFE

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, PTFE Filled
Manufacturer Techmer ES
Trade Name Plaslube®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Plaslube® AC-80/TF/15 Acetal (Copolymer), 15% PTFE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Plaslube polytetrafluoroethylene (PTFE) lubricated acetal copolymer grades offer additional wear and friction performance over neat acetal. Typical applications include bearings, slides and small gears.
Physical Properties Metric English Comments
Density 1.49 g/cc
0.0538 lb/in³
ASTM D792
Water Absorption 0.23 %
0.23 %
24 hrs. ASTM D570
Linear Mold Shrinkage 0.020 cm/cm

@Thickness 3.17 mm
0.020 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 43.4 MPa
6300 psi
ASTM D638
Flexural Yield Strength 66.2 MPa
9600 psi
ASTM D790
Flexural Modulus 2.14 GPa
310 ksi
ASTM D790
Izod Impact, Notched 0.481 J/cm

@Thickness 3.17 mm
0.900 ft-lb/in

@Thickness 0.125 in
ASTM D256
Coefficient of Friction, Dynamic 0.16
0.16
Coefficient of Friction, Static 0.080
0.080
K (wear) Factor 201 x 10-8 mm³/N-M
100 x 10-10 in³-min/ft-lb-hr
Thrust washer at 2000 PV
Limiting Pressure Velocity 0.420 MPa-m/sec
12000 psi-ft/min
at 100 FPM, ambient temperature, thrust washer.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
215 °F
ASTM D648
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved