Techmer ES Plaslube® J-1305/30/TF/15 BK5011 PPS

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled
Manufacturer Techmer ES
Trade Name Plaslube®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Plaslube® J-1305/30/TF/15 BK5011 PPS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D792
Water Absorption 0.020 %
0.020 %
24 Hrs; ASTM D570
Linear Mold Shrinkage 0.0010 - 0.0020 cm/cm
0.0010 - 0.0020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 131 MPa
19000 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Strength 193 MPa
28000 psi
ASTM D790
Flexural Modulus 11.0 GPa
1600 ksi
ASTM D790
Izod Impact, Notched 0.801 J/cm
1.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Flammability, UL94 V-0

@Thickness 3.17 mm
V-0

@Thickness 0.125 in
V-0

@Thickness 1.59 mm
V-0

@Thickness 0.0625 in