Techmer ES Plaslube® NY-1/MS/5 BK223 PA66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, MoS2 Filled
Manufacturer Techmer ES
Trade Name Plaslube®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Plaslube® NY-1/MS/5 BK223 PA66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc
1.16 g/cc
ASTM D792
Water Absorption 0.90 %
0.90 %
24 Hrs; ASTM D570
Linear Mold Shrinkage 0.010 - 0.012 cm/cm
0.010 - 0.012 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength at Break 86.2 MPa
12500 psi
ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Flexural Strength 124 MPa
18000 psi
ASTM D790
Flexural Modulus 3.34 GPa
485 ksi
ASTM D790
Izod Impact, Notched 0.427 J/cm
0.800 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 93.3 °C
200 °F
ASTM D648