Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES Plastiblend® ABS 8007

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer Techmer ES
Trade Name Plastiblend®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Plastiblend® ABS 8007.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFeatures: General Purpose and High FlowInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0050 cm/cm

@Thickness 3.17 mm
0.0050 in/in

@Thickness 0.125 in
ASTM D955
Melt Flow 10 g/10 min

@Load 3.80 kg,
Temperature 230 °C
10 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
35 g/10 min

@Load 10.0 kg,
Temperature 220 °C
35 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 102
102
ASTM D785
Tensile Strength, Yield 33.1 MPa
4800 psi
ASTM D638
Elongation at Break 2.4 %
2.4 %
ASTM D638
Flexural Strength 64.8 MPa
9400 psi
ASTM D790
Flexural Modulus 2.34 GPa
340 ksi
ASTM D790
Izod Impact, Notched 0.801 J/cm

@Thickness 3.17 mm,
Temperature -30.0 °C
1.50 ft-lb/in

@Thickness 0.125 in,
Temperature -22.0 °F
ASTM D256
0.854 J/cm

@Thickness 3.17 mm,
Temperature -17.8 °C
1.60 ft-lb/in

@Thickness 0.125 in,
Temperature 0.000 °F
ASTM D256
2.40 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
4.50 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 88.9 °C
192 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
167 °F
Unannealed; ASTM D648
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved