Material Notes:
Availability: North AmericaForms: PelletsFeatures: CopolymerAppearance: Clear/TransparentInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0060 cm/cm

@Thickness 3.17 mm
0.0060 in/in

@Thickness 0.125 in
ASTM D955
Melt Flow 9.0 g/10 min

@Load 3.80 kg,
Temperature 230 °C
9.0 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 112
112
ASTM D785
Tensile Strength, Yield 51.0 MPa
7400 psi
ASTM D638
Elongation at Break 6.0 %
6.0 %
ASTM D638
Flexural Strength 78.6 MPa
11400 psi
ASTM D790
Flexural Modulus 2.34 GPa
340 ksi
ASTM D790
Izod Impact, Notched 0.481 J/cm

@Thickness 3.17 mm,
Temperature 0.000 °C
0.900 ft-lb/in

@Thickness 0.125 in,
Temperature 32.0 °F
ASTM D256
1.07 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
2.00 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
194 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 82.8 °C
181 °F
Unannealed; ASTM D648
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Users viewing this material also viewed the following: