Techmer ES Plastiblend® PC/ASA FR1508 UV

Category Polymer , Thermoplastic , ASA Polymer , Polycarbonate (PC) , Polycarbonate/ASA Alloy, Unreinforced
Manufacturer Techmer ES
Trade Name Plastiblend®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Plastiblend® PC/ASA FR1508 UV.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsAdditive: Flame Retardant and UV StabilizerFeatures: Flame Retardant, Good UV Resistance and Halogen FreeInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ASTM D792
Water Absorption 0.24 %

@Time 86400 sec
0.24 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0045 cm/cm

@Thickness 3.17 mm
0.0045 in/in

@Thickness 0.125 in
ASTM D955
Melt Flow 45 g/10 min

@Load 5.00 kg,
Temperature 260 °C
45 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
ASTM D785
Tensile Strength, Yield 64.8 MPa
9400 psi
ASTM D638
Elongation at Break 27 %
27 %
ASTM D638
Elongation at Yield 3.5 %
3.5 %
ASTM D638
Flexural Yield Strength 84.1 MPa
12200 psi
ASTM D790
Flexural Modulus 2.59 GPa
375 ksi
ASTM D790
Izod Impact, Notched 1.87 J/cm

@Thickness 3.17 mm
3.50 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 72.0 µm/m-°C
40.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 98.9 °C
210 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 96.1 °C
205 °F
Unannealed; ASTM D648
Flammability, UL94 V-0
V-0