Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES Statiblend® 02010 MB Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Techmer ES
Trade Name Statiblend®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Statiblend® 02010 MB Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified FillerReinfor.Features: ConductiveAppearance: BlackTPCI# 9125116Information provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 0.955 g/cc
0.0345 lb/in³
ASTM D792
Melt Flow 6.0 g/10 min

@Load 10.0 kg,
Temperature 200 °C
6.0 g/10 min

@Load 22.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 19.3 MPa
2800 psi
ASTM D638
Elongation at Break 50 %
50 %
ASTM D638
Flexural Strength 27.6 MPa
4000 psi
ASTM D790
Flexural Modulus 0.965 GPa
140 ksi
ASTM D790
Izod Impact, Notched 3.20 J/cm

@Thickness 3.17 mm
6.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched NB

@Thickness 3.17 mm
NB

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 68.4 µm/m-°C
38.0 µin/in-°F
ASTM D696
Electrical Properties Metric English Comments
Volume Resistivity 1000 ohm-cm
1000 ohm-cm
ASTM D257
Surface Resistance 100 ohm - 1e+05
100 ohm - 1e+05
ASTM D257
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved