Techmer ES Statiblend® ABS E AS

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer Techmer ES
Trade Name Statiblend®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Statiblend® ABS E AS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsAdditive: AntistaticFeatures: AntistaticInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ASTM D792
Melt Flow 1.0 g/10 min

@Load 3.80 kg,
Temperature 230 °C
1.0 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength, Yield 37.9 MPa
5500 psi
ASTM D638
Elongation at Yield 10 %
10 %
ASTM D638
Flexural Yield Strength 69.6 MPa
10100 psi
ASTM D790
Flexural Modulus 2.28 GPa
330 ksi
ASTM D790
Izod Impact, Notched 2.67 J/cm

@Thickness 3.17 mm
5.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched NB

@Thickness 3.17 mm
NB

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 68.4 µm/m-°C
38.0 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
215 °F
Unannealed; ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+10 ohm-cm
1.00e+10 ohm-cm
ASTM D257
Surface Resistance 1.00e+9 ohm
1.00e+9 ohm
ASTM D257