Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified FillerReinforAdditive: Impact ModifierFeatures: Conductive and Impact ModifiedUL File Number: E157318TPCI# 1039101Information provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.010 cm/cm

@Thickness 3.17 mm
0.010 in/in

@Thickness 0.125 in
ASTM D955
Melt Flow 1.1 g/10 min

@Load 10.0 kg,
Temperature 230 °C
1.1 g/10 min

@Load 22.0 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 89
89
ASTM D785
Tensile Strength, Yield 75.8 MPa
11000 psi
ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Flexural Strength 110 MPa
16000 psi
ASTM D790
Flexural Modulus 3.45 GPa
500 ksi
ASTM D790
Izod Impact, Notched 0.747 J/cm

@Thickness 3.17 mm
1.40 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 121 °C
250 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+6 - 1.00e+9 ohm-cm
1.00e+6 - 1.00e+9 ohm-cm
ASTM D257
Surface Resistance 1.00e+6 - 1.00e+9 ohm
1.00e+6 - 1.00e+9 ohm
ASTM D257