Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES Statiblend® PPS GF40 EC BK 40% Glass Filled

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler , Polyphenylene Sulfide (PPS), Stainless Steel Fiber
Manufacturer Techmer ES
Trade Name Statiblend®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Statiblend® PPS GF40 EC BK 40% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 40% Filler by WeightFeatures: Semi ConductiveUL File Number: E157318Appearance: BlackInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.67 g/cc
0.0603 lb/in³
ASTM D792
Water Absorption 0.60 %

@Time 86400 sec
0.60 %

@Time 24.0 hour
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 123
123
ASTM D785
Tensile Strength, Yield 131 MPa
19000 psi
ASTM D638
Elongation at Yield 2.5 %
2.5 %
ASTM D638
Flexural Yield Strength 165 MPa
24000 psi
ASTM D790
Flexural Modulus 13.8 GPa
2000 ksi
ASTM D790
Izod Impact, Notched 0.801 J/cm

@Thickness 3.17 mm
1.50 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 19.8 µm/m-°C
11.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 257 °C
495 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 260 °C
500 °F
Unannealed; ASTM D648
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1000 ohm-cm
1000 ohm-cm
ASTM D257
Surface Resistance 1e+05
1e+05
ASTM D257