Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Technetics Group Amicon™ Acetal Homopolymer  (Unverified Data**)

Category Polymer , Thermoplastic , Acetal (POM)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Technetics Group Amicon™ Acetal Homopolymer  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Technetics Group (formerly Plastomer Technologies)
Physical Properties Metric English Comments
Specific Gravity 1.41 g/cc
1.41 g/cc
ASTM D792
Water Absorption 0.20 %
0.20 %
24 hours; ASTM D570 (2)
Water Absorption at Saturation 0.90 %
0.90 %
ASTM D570 (2)
Mechanical Properties Metric English Comments
Hardness, Shore D 86
86
ASTM D2240
Tensile Strength, Ultimate 75.8 MPa
11000 psi
ASTM D638
Elongation at Break 30 %
30 %
ASTM D638
Modulus of Elasticity 3.10 GPa
450 ksi
ASTM D638
Flexural Strength 89.6 MPa
13000 psi
ASTM D790
Flexural Modulus 3.10 GPa
450 ksi
ASTM D790
Compressive Strength 110 MPa
16000 psi
ASTM D695
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D256 type "A"
Coefficient of Friction 0.25
0.25
ASTM PTM 55007
K (wear) Factor 403 x 10-8 mm³/N-M
200 x 10-10 in³-min/ft-lb-hr
QTM 55010
Limiting Pressure Velocity 0.0946 MPa-m/sec
2700 psi-ft/min
4:1 safety factor
Thermal Properties Metric English Comments
CTE, linear 84.6 µm/m-°C

@Temperature 100 °C
47.0 µin/in-°F

@Temperature 212 °F
ASTM E-831 (TMA)
Maximum Service Temperature, Air 82.2 °C
180 °F
Flammability, UL94 HB

@Thickness 3.17 mm
HB

@Thickness 0.125 in
ASTM UL-94
Electrical Properties Metric English Comments
Dielectric Constant 3.7

@Frequency 1e+6 Hz
3.7

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 17.7 kV/mm
450 kV/in
ASTM D149
Dissipation Factor 0.0050

@Frequency 1e+6 Hz
0.0050

@Frequency 1e+6 Hz
ASTM D150