Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Teijin Multilon TN-7100F Filler Reinforced Type, Halogen-Free Flame Resistant PC/ABS Polymer Alloy

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate (PC)
Manufacturer Teijin
Trade Name Multilon
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teijin Multilon TN-7100F Filler Reinforced Type, Halogen-Free Flame Resistant PC/ABS Polymer Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Halogen-free flame retardant PC/ABS polymer alloy, and is also antimony-free. High stiffness and flowability realize the thin wall of large-scale business machine chassis.Information provided by Teijin Chemicals Ltd.
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
ISO 1183
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm

@Thickness 4.00 mm
0.0040 - 0.0060 in/in

@Thickness 0.157 in
Linear Mold Shrinkage, Transverse 0.0040 - 0.0060 cm/cm

@Thickness 4.00 mm
0.0040 - 0.0060 in/in

@Thickness 0.157 in
Mechanical Properties Metric English Comments
Tensile Strength at Break 46.0 MPa
6670 psi
50mm/min; ISO 527
Tensile Strength, Yield 62.0 MPa
8990 psi
50mm/min; ISO 527
Elongation at Break 50 %
50 %
50mm/min; ISO 527
Elongation at Yield 2.0 %
2.0 %
50mm/min; ISO 527
Tensile Modulus 3.30 GPa
479 ksi
1mm/min; ISO 527
Flexural Strength 94.0 MPa
13600 psi
2mm/min; ISO 178
Flexural Modulus 3.20 GPa
464 ksi
2mm/min; ISO 178
Charpy Impact Unnotched NB
NB
ISO 179
Charpy Impact, Notched 2.20 J/cm²
10.5 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
CTE, linear 60.0 µm/m-°C

@Temperature 20.0 °C
33.3 µin/in-°F

@Temperature 68.0 °F
ISO 11359
CTE, linear, Transverse to Flow 70.0 µm/m-°C

@Temperature 20.0 °C
38.9 µin/in-°F

@Temperature 68.0 °F
ISO 11359
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °C
199 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 83.0 °C
181 °F
ISO 75
Vicat Softening Point 96.0 °C
205 °F
50°C/hr, 50N; ISO 306
Flammability, UL94 V-1

@Thickness 1.00 mm
V-1

@Thickness 0.0394 in
V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
5VB

@Thickness 1.80 mm
5VB

@Thickness 0.0709 in
Electrical Properties Metric English Comments
Surface Resistance 1.00e+16 ohm
1.00e+16 ohm
IEC 60093
Users viewing this material also viewed the following: