Teknor Apex APEX® 130 Polyvinyl Chloride, Flexible

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade , PVC, Wire and Cable Grade
Manufacturer Teknor Apex Company
Trade Name APEX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex APEX® 130 Polyvinyl Chloride, Flexible.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Notes: 80°C Jacket; RoHS CompliantFeatures: Sunlight Resistant (720 hours); Good UV Resistance Uses: Appliance Wire Jacketing; Building Wire Jacketing; Flexible Cord Jacketing; Wire and Cable Applications Agency Ratings: UL QMTT2 .E73402Forms: Pellets Wire Types: AWM; SJTW; SRDT; STW; SVT; UF; UL Style 2835 Processing Method: Extrusion Additional Information: UL Recognized Component as PVC 300 Hour Sunlight Resistant Jacket Compound, QMTT2 UL Recognized as PVC 720 Hour Sunlight Resistant Insulation and Jacket Compounds, QMTT2 1/32 in wall Temperature Rating: 80°C UL Recognized Insulation: No Ultimate Elongation Retained, UL 1581, Oven Aged, 7 days, 113°C: 89% Tensile Strength Retained, UL 1581, Oven Aged, 7 days, 113°C: 103%Information Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.37 g/cc
1.37 g/cc
ASTM D792
Melt Flow 1.60 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.60 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
10 seconds; ASTM D2240
Tensile Strength at Break 15.9 MPa
2300 psi
ASTM D638
Elongation at Break 350 %
350 %
ASTM D638
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 80.0 °C
176 °F
Continuous Use; ASTM D794
Brittleness Temperature -30.0 °C
-22.0 °F
ASTM D746
Oxygen Index 22 %
22 %
ASTM D2863
Descriptive Properties Value Comments
Appearance Opaque