Teknor Apex APEX® 89-P180-B Polyvinyl Chloride, Flexible

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade , PVC, Wire and Cable Grade
Manufacturer Teknor Apex Company
Trade Name APEX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex APEX® 89-P180-B Polyvinyl Chloride, Flexible.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Notes: 80°C Jacket; RoHS CompliantFeatures: Flame Retardant; Low gloss; Low Temperature Flexibility Uses: Cable JacketingAgency Ratings: UL 62 Forms: Pellets Wire Types: SJT; ST; SVTInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore C 73
73
10 seconds; ASTM D2240
Tensile Strength at Break 14.7 MPa
2130 psi
ASTM D638
Elongation at Break 310 %
310 %
ASTM D638
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 80.0 °C
176 °F
Continuous Use; ASTM D794
Brittleness Temperature -33.0 °C
-27.4 °F
ASTM D746
Oxygen Index 28 %
28 %
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity 1.60e+11 ohm-cm
1.60e+11 ohm-cm
ASTM D257
Descriptive Properties Value Comments
Appearance Opaque