Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Teknor Apex Beetle® MDF2 Nylon 6, 30% Short Glass Fiber Reinforced, Dry

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled , Nylon 6, Glass Fiber Filled, Flame Retardant
Manufacturer Teknor Apex Company
Trade Name Beetle®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Beetle® MDF2 Nylon 6, 30% Short Glass Fiber Reinforced, Dry.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Notes: MDF2 is a heat stabilized 30% glass fiber reinforced nylon 6 that offers good mechanical performance coupled with good surface finish. Features: Heat Stabilized; Good Surface Finish Processing Method: Injection Molding Forms: PelletsAdditive: Heat Stabilizer Injection Notes: No drying is necessary unless the material has been exposed to air for longer than 3 hours; Back Pressure: Low; Injection Pressure; High; Injection Rate: FastInformation Provided by Teknor Apex
Thermal Properties Metric English Comments
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Processing Properties Metric English Comments
Rear Barrel Temperature 240 - 280 °C
464 - 536 °F
Middle Barrel Temperature 240 - 280 °C
464 - 536 °F
Front Barrel Temperature 240 - 280 °C
464 - 536 °F
Melt Temperature <= 300 °C
<= 572 °F
Processing Temperature
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 2 hour
2 hour
Screw Speed 50 - 200 rpm
50 - 200 rpm