Teknor Apex Chemlon® ALF20 Nylon 66, Unreinforced

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced
Manufacturer Teknor Apex Company
Trade Name Chemlon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Chemlon® ALF20 Nylon 66, Unreinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Notes: ALF20 is a self-lubricating grade of nylon 66 containing PTFE and Silicone. It offers outstanding surface wear characteristics of molded parts. It is suitable for applications such as bearings and mechanical parts. Features: Good Wear Resistance; Low Friction; Self Lubricating Processing Method: Injection Molding Forms: Pellets Uses: Bearings; Machine/Mechanical parts Injection Notes: No drying is necessary unless the material has been exposed to air for longer than 3 hours; Back Pressure: Low; Injection Pressure: High; Injection Rate: FastInformation Provided by Teknor Apex
Mechanical Properties Metric English Comments
K (wear) Factor 24.2 x 10-8 mm³/N-M
12.0 x 10-10 in³-min/ft-lb-hr
ASTM D3702
Processing Properties Metric English Comments
Rear Barrel Temperature 270 - 290 °C
518 - 554 °F
Middle Barrel Temperature 270 - 290 °C
518 - 554 °F
Front Barrel Temperature 270 - 290 °C
518 - 554 °F
Melt Temperature 265 °C
509 °F
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 2 hour
2 hour