Material Notes:
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, General Purpose, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather ResistanceUses- Automotive ApplicationsFootwear, Tubing, Gaskets, Weatherstripping, hose, Wheels, SealsForms-PelletsProcessing-Extrusion, Injection MoldingInformation provided by Teknor Apex Company
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
23°C; ASTM D792
Linear Mold Shrinkage 0.010 - 0.025 cm/cm
0.010 - 0.025 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
15 seconds; ASTM D2240
Tensile Strength, Yield 3.79 MPa
550 psi
100%; ASTM D412
11.7 MPa
1700 psi
ASTM D412
Elongation at Break 380 %
380 %
ASTM D412
Tear Strength 28.0 kN/m
160 pli
Die C; ASTM D624
Compression Set 23 %
23 %
73°F, 22 hr.; ASTM D395
55 %
55 %
158°F, 22 hr.; ASTM D395
Thermal Properties Metric English Comments
Brittleness Temperature -56.1 °C
-69.0 °F
ASTM D746
Processing Properties Metric English Comments
Rear Barrel Temperature 171 - 188 °C
340 - 370 °F
Middle Barrel Temperature 171 - 188 °C
340 - 370 °F
Front Barrel Temperature 171 - 188 °C
340 - 370 °F
Mold Temperature 23.9 - 51.7 °C
75.0 - 125 °F
Back Pressure 0.345 - 1.03 MPa
50.0 - 150 psi
Descriptive Properties Value Comments
Screw Compression Ratio 2:1-3:1
Screw L/D Ratio 20:1- 24:1
Suggested Max Regrind, % 20
Users viewing this material also viewed the following: