Material Notes:
Notes: RoHS Compliant Features: Flame Retardant; Halogen Free Uses: Communication Wire Jacketing; Electronic Cable Jacketing; Security Cable Jacketing; Plenum Cable JacketingAgency Ratings: IEC Unspecified Rating; ICEA Unspecified Rating; UL QMTT2 .E200337 Processing Method: Extrusion Forms: Pellets Additional Information: Ultimate Elongation Retained, UL 1581, Oven Aged, 7 days, 100°C: 78% Tensile Strength Retained, UL 1581, Oven Aged, 7 days, 100°C: 113% Ultimate Elongation Retained, UL 1581, Oven Aged, 7 days, 113°C: 74% Tensile Strength Retained, UL 1581, Oven Aged, 7 days, 113°C: 108% Ultimate Elongation Retained, UL 1581, Oven Aged, 7 days, 125°C: 73% Tensile Strength Retained, UL 1581, Oven Aged, 7 days, 125°C: 116% Ultimate Elongation Retained, UL 1581, Oven Aged, 7 days, 136°C: 72% Tensile Strength Retained, UL 1581, Oven Aged, 7 days, 136°C: 109% Acid Gas, MIL-C-24643: < 5.0 mg Acidity of Gases, IEC-754-2: < 6.0 pH Conductivity: < 2.0 µS/cm Smoke Index, NES-711: < 10.0 Toxicity Index, NES-713: 0.085 Acid Gas, MIL-C-24643: < 5.0 mg Acidity of Gases, IEC-754-2: < 6.0 pH Conductivity: < 2.0 µS/cm Smoke Index, NES-711: < 10.0 Toxicity Index, NES-713: < 1.0 Cone Calorimeter at 50 kW/m2, Peak Heat Release Rate: 154 kW/m2 Cone Calorimeter at 50 kW/m2, Total Heat Released: 157 MJ/m2 Cone Calorimeter at 50 kW/m2, Peak Smoke: 0.8 1/m Cone Calorimeter at 50 kW/m2, Time to Sustained Ignition: 138 secInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.49 g/cc
1.49 g/cc
ASTM D792
Melt Flow 1.50 g/10 min

@Load 10.0 kg,
Temperature 190 °C
1.50 g/10 min

@Load 22.0 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 53
53
10 seconds; ASTM D2240
Tensile Strength at Break 14.3 MPa
2070 psi
ASTM D638
Elongation at Break 140 %
140 %
ASTM D638
Thermal Properties Metric English Comments
Brittleness Temperature -40.0 °C
-40.0 °F
ASTM D746
Oxygen Index 44 %
44 %
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity 9.70e+14 ohm-cm
9.70e+14 ohm-cm
ASTM D257
Dielectric Constant 3.66

@Frequency 1000 Hz
3.66

@Frequency 1000 Hz
ASTM D150
Dissipation Factor 0.0020

@Frequency 1000 Hz
0.0020

@Frequency 1000 Hz
ASTM D150
Descriptive Properties Value Comments
Appearance Opaque