Teknor Apex Monprene® MP 1870 Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Teknor Apex Company
Trade Name MONPRENE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Monprene® MP 1870 Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Monprene® TPE gels are softer than the shore A range of hardness. Monprene® TPE gels are high strength and high flow elastomers that may be used in the overmolding processes on polyolefin substrates. Monprene® TPE gels are recommended for applications where very soft tactile feel and strength are required, such as cushions or padding between hard substrates and personal contact.Information Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 0.880 g/cc
0.880 g/cc
ASTM D792
Melt Flow 15.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
15.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 65
65
ASTM D2240
Tensile Strength at Break 4.14 MPa
600 psi
ASTM D412
Tensile Strength, Yield 0.689 MPa

@Strain 300 %
100 psi

@Strain 300 %
ASTM D412
Elongation at Break 600 %
600 %
ASTM D412
Copyright © lookpolymers.com All Rights Reserved