Teknor Apex Sinelec CCB2095 Specialty Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Molded, Unreinforced
Manufacturer Teknor Apex Company
Trade Name Sinelec
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Sinelec CCB2095 Specialty Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Features: Electrically Conductive Forms: Pellets Processing Method: Injection MethodInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
ASTM D955
Melt Flow 1.50 g/10 min

@Load 10.0 kg,
Temperature 230 °C
1.50 g/10 min

@Load 22.0 lb,
Temperature 446 °F
ASTM D1238
15.0 g/10 min

@Load 21.6 kg,
Temperature 230 °C
15.0 g/10 min

@Load 47.6 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 35.0 MPa
5080 psi
ASTM D638
Elongation at Break 19 %
19 %
ASTM D638
Flexural Strength 36.0 MPa
5220 psi
ASTM D790
Flexural Modulus 2.00 GPa
290 ksi
ASTM D790
Izod Impact, Notched 0.400 J/cm

@Temperature 22.8 °C
0.750 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C
185 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1e+05
1e+05
ASTM D257
Surface Resistance 1e+05
1e+05
ASTM D257