Material Notes:
Availability: Asia Pacific Features: High Strength Uses: Electrical/Electronic Applications < Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 83
83
ASTM D2240
Tensile Strength, Yield 13.53 MPa
1962 psi
Change in tensile strength after 168 hours at 212°F; ASTM D638
15.0 MPa
2180 psi
9.8 in/min; ASTM D638
Elongation at Break 200 %
200 %
Change after 168 hours at 212°F; ASTM D638
250 %
250 %
9.8 in/min; ASTM D638
Electrical Properties Metric English Comments
Volume Resistivity 5.00e+13 ohm-cm

@Temperature 20.0 °C
5.00e+13 ohm-cm

@Temperature 68.0 °F
BS 2782