Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Teknor Apex TEKRON® 4300LM-P88-1 Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Teknor Apex Company
Trade Name TEKRON®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex TEKRON® 4300LM-P88-1 Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Teknor Apex Company
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
+/- 0.02; ASTM D792
Linear Mold Shrinkage, Flow 0.016 cm/cm
0.016 in/in
24 hours
0.019 cm/cm
0.019 in/in
24 hours + 30 min at 93°C
Linear Mold Shrinkage, Transverse 0.015 cm/cm
0.015 in/in
24 hours
0.016 cm/cm
0.016 in/in
24 hours + 30 min. at 93°C
Melt Flow 7.08 g/10 min

@Load 2.16 kg,
Temperature 230 °C
7.08 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 91
91
15 second delay. +/-3; ASTM D2240
Tensile Strength, Yield 8.508 MPa
1234 psi
ASTM D412
Elongation at Break 630 %
630 %
ASTM D412
Elongation at Yield 29 %
29 %
ASTM D412
100% Modulus 0.00614 GPa
0.890 ksi
ASTM D412
300% Modulus 0.00731 GPa
1.06 ksi
ASTM D412
Flexural Modulus 0.138 GPa
20.0 ksi
ASTM D790
Tear Strength 65.0 kN/m
371 pli
Die C; ASTM D1004
Thermal Properties Metric English Comments
CTE, linear 147 µm/m-°C

@Temperature 20.0 °C
81.7 µin/in-°F

@Temperature 68.0 °F
CTE, linear, Transverse to Flow 132 µm/m-°C

@Temperature 20.0 °C
73.3 µin/in-°F

@Temperature 68.0 °F
Brittleness Temperature <= -65.0 °C
<= -85.0 °F
ASTM D746
Flame Spread 50.8 mm/min
2.00 in/min
Pass: Burn Rate- Max 100; FMVSS 302
Descriptive Properties Value Comments
Fogging 90, 3 hours at 100°C, cooling plate 21°C, value after 1 hour. (SAE-J1756)