Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Teknor Apex Telcar® TL-1934E Styrenic Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Teknor Apex Company
Trade Name TELCAR®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Telcar® TL-1934E Styrenic Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Uses: Appliance Wire Insulation; Cable Jacketing; Flexible Cord Insulation; Wire and Cable Applications; Wire Jacketing Agency Ratings: UL 1581 Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed: 30 to 100 rpmInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.31 g/cc
1.31 g/cc
ASTM D792
Melt Flow 18.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
18.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 83
83
ASTM D2240
Tensile Strength at Break 9.5113 MPa
1379.5 psi
Change in tensile strength in air after 168 hours at 316°F; ASTM D573
10.26 MPa
1488 psi
Change in tensile strength in air after 3600 hours at 268°F; ASTM D573
10.7 MPa
1550 psi
20 in/min; ASTM D412
Elongation at Break 529.2 %
529.2 %
Change in tensile elongation in air after 3600 hours at 268°F; ASTM D573
535.5 %
535.5 %
Change in tensile elongation in air after 168 hours at 316°F; ASTM D573
630 %
630 %
20 in/min; ASTM D412
Thermal Properties Metric English Comments
Brittleness Temperature -59.0 °C
-74.2 °F
ASTM D746
Flammability, UL94 V-0

@Thickness 1.52 mm
V-0

@Thickness 0.0600 in
QMFZ2.E54709; QMTT2.E73402
Oxygen Index 26 %
26 %
ASTM D2863
Electrical Properties Metric English Comments
Dielectric Constant 2.4
2.4
ASTM D150
Dielectric Strength 35.4 kV/mm
900 kV/in
ASTM D419
Dissipation Factor 0.0040
0.0040
ASTM D150
Processing Properties Metric English Comments
Rear Barrel Temperature 171 - 193 °C
340 - 380 °F
Middle Barrel Temperature 177 - 199 °C
350 - 390 °F
Front Barrel Temperature 182 - 204 °C
360 - 400 °F
Nozzle Temperature 188 - 210 °C
370 - 410 °F
Zone 1 166 - 188 °C
330 - 370 °F
Zone 2 171 - 193 °C
340 - 380 °F
Zone 3 177 - 199 °C
350 - 390 °F
Zone 5 182 - 204 °C
360 - 400 °F
Die Temperature 190 - 210 °C
374 - 410 °F
Melt Temperature 188 - 210 °C
370 - 410 °F
Processing Temperature
Mold Temperature 25.0 - 65.6 °C
77.0 - 150 °F
Injection Pressure 1.38 - 6.89 MPa
200 - 1000 psi
Back Pressure 0.172 - 0.345 MPa
25.0 - 50.0 psi
Cushion 0.381 - 2.54 cm
0.150 - 1.00 in
Screw Speed 50 - 100 rpm
50 - 100 rpm
Descriptive Properties Value Comments
Appearance Opaque